Welding Defect Classification Based on Convolution Neural Network (CNN) and Gaussian Kernel

2017-09-30IEEE 2017Unverified0· sign in to hype

Agus Khumaidi1, Eko Mulyanto Yuniarno1, 2, Mauridhi Hery Purnomo1, 2 1 Department of Electrical Engineering, 2 Department of Computer Engineering, Institut Teknologi Sepuluh Nopember Surabaya, Indonesia

Unverified — Be the first to reproduce this paper.

Reproduce

Abstract

Visual inspection process for weld defects still manually operated by human vision, so the result of the test still highly subjective. In this research, the visual inspection process will be done through image processing on the image sequence to make data accuracy more better. CNN as one of the image processing technique can determine the feature automatically which is suitable for this problem in order to classify the variation of each weld defect pattern. Classification using Convolution Neural Network (CNN) consist of two stages: extraction image using image convolution and image classification using neural network. Gaussian kernel used for blurring image, it helps the extraction of images without losing the main information from the original image, this filter also minimize the occurrence of interference or noise. Results of the classification used to get the category of weld defects with high accuracy as a variable of a weld inspection process whether the weld is pass the standard or not. The proposed system has obtained classification with validation accuracy of 95.83% for four different type of welding defect. The data input of this research is the result of images captured by a webcam.

Tasks

Reproductions